ASTM A269 vexillum specificatio est pro sessili et austenitico incorrupta ferro tubingo iuncta pro corrosione generali resistendi et demissa vel alta temperaturae officia. ASTM A249 norma specificatio est pro ferro austenitico iuncta bullientis, superheatri, caloris commutatoris et fistulae condensoris. ASTM A213 norma specificatio est ob inconsutilem ferriticum et austeniticum alloy-ferrum boiler, superheater, et fistulae caloris commutatoris. Differentiae inter A269, A249 et A213 iacent in signis specificis quae pro ferro incorrupta Tubing repraesentant.
STANDARD ASTMA249 ASTM A269 ASTMA270 ASTM213
Standard | Tolerantia extra Diameter (mm) | Muri crassitudine% | Longitudo Tolerantia (mm) | ||
ASTM A249 | <25.0 | +0.10 -0.11 | ±10% | ||
≥25.0-≤40.0 | ±0.15 | ||||
>40.0-<50.0 | ±0.20 | OD<50.8 | +3.0-0.0 | ||
≥50.0~<65.0 | ±0.25 | ||||
≥65.0-<75.0 | ±0.30 | ||||
≥75.0~<100.0 | ±0.38 | OD≥50.8 | +5.0-0.0 | ||
≥100~≤200.0 | +0.38 -0.64 | ||||
>200.0-≤225.0 | +0.38 -1.14 | ||||
ASTM A269 | <38.1 | ±0.13 | |||
≥38.1~<88.9 | ±0.25 | ||||
≥88.9-<139.7 | ±0.38 | ±15.0% | OD <38.1 | +3.2-0.0 | |
≥139.7~<203.2 | ±0.76 | ±10.0% | 0D ≥38.1 | +4.0-0.0 | |
≥203.2-<304.8 | ±1.01 | ||||
≥304.8-<35.6 | ±1.26 | ||||
ASTMA270 | ≤25.4 | ±0.13 | ±10% | +10-0.0 | |
>25.4-≤50.8 | ±0.20 | ||||
>50.8~≤62 | ±0.25 | ||||
>76.2- ≤101.6 | ±0.38 | ||||
>101.6~<139.7 | ±0.38 | ||||
≥139.7-203.2 | ±0.76 | ||||
≥203 2~≤304.8 | ±1.27 | ||||
ASTM213 | D<25.4 | ± 0.10 | +20/0 | +3.0/0 | |
25.4~38.1 | ±0.15 | ||||
38.1~50.8 | ±0.20 | ||||
50.8~63.5 | ±0.25 | +22/0 | +5.0/0 | ||
63.5~76.2 | ±0.30 | ||||
76.2~ 101.6 | ±0.38 | ||||
101.6~ 190.5 | +0.38/-0.64 | ||||
190.5~228.6 | +0.38/-1.14 |